API 650 - Section -6 (Fabrication) Flashcards

1
Q

When material requires straightening, the work shall be done by ,,,,,,, or another,,,,, method prior to any layout or shaping

A

pressing, noninjurious

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
2
Q

Heating or hammering is ,,,,,, unless the material is maintained at forging during straightening

A

not permissible

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
3
Q

Attachments that will be welded to the pressure boundary shall not have a ,,,, or ,,,,, coating in the weld area within ,,,,,, of the weld.

A
zinc, cadmium
12 mm (0.5 in.)
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
4
Q

Shearing shall be limited to plates ,,,,,, thick used for butt-welded joints and to plates ,,,,,,,thick used for lap-welded joints.

A

≤ 10 mm (3/8 in.)

≤ 16 mm (5/8 in.)

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
5
Q

With the Purchaser’s approval, the shearing limitation on plates used for butt-welded joints may be increased to a
thickness ,,,,,,,,,

A

≤ 16 mm (5/8 in.)

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
6
Q

The Purchaser’s inspector shall be permitted ,,,,,,to all parts of the Manufacturer’s plant that are concerned with the contract whenever any work under the contract is being performed.

A

free entry

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
7
Q

If a lamination is visually detected, the Manufacturer shall ultrasonically examine the area to determine the extent of the laminations and shall ,,,, the plate or make ,,,

A

reject

repairs

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
8
Q

For laminations found not exceeding ,,,,,,, in length or ,,,, in depth, repairs may be made by edge gouging and re welding to seal the lamination

A
75 mm (3 in.)
25 mm (1 in.)
How well did you know this?
1
Not at all
2
3
4
5
Perfectly