Percentages Flashcards
NDE - Limits of RT Film Density of weld as compared to IQI
-15 to +30% ASME V: T-282.2.a.1
Design - Mill Tolerance of Seamless Pipe
-12.5% 574: 4.1.1.3
Pipe Class - % of H2S in process to classify as Class 1 Pipe
Equal to or > 3% 570: 6.3.4.2.c
NDE - % of welds to RT when fabricating Normal Service Pipe
5% B31.3: 341.4.1.b.1
NDE - % of welds to VT when fabricating Normal Service Pipe
5% B31.3: 341.4.1.a.2
NDE - % of welds to Brinnell after PWHT in furnace (if BHN are required)
10% B31.3: 331.1.7.a
NDE – Overlap with a UT scan, % of transducer diameter
10% 574: 10.2.1.4.3
AI – Amount of time inspector must be involved in inspection activities - required to maintain API 570 certification
20% 570: A.3.2
Mtls – Amount of nickel required for a material to be considered a nickel alloy
> 30% 571: 3.1.15
NDE - % of welds to Brinnell after local PWHT (if BHN is reqd)
100% B31.3: 331.1.7.a
NDE - % of Visual & RT required when fabricating Severe Cyclic Pipe
100% B31.3: 341.4.3.a.1/b
Testing - Pneumatic test pressure, % of design pressure
110% B31.3: 345.5.4
Testing - Leak test pressure of underground pipe, % of operating pressure
110% 570: 9.3.7
PRV - Maximum set pressure for thermal relief valves, % of design pressure
120% B31.3: 322.6.3.b.2