NDE - Limits of RT Film Density of weld as compared to IQI (range)
-15 to +30%
V: T-282.2.a.1
Mtls – Max chrome content to be considered Low Alloy steel
9%
571: 2.1.11
NDE - UT Corrosion Mapping. Minimum overlap of Transducer
10%
575: A.2
Mtls – Minimum chrome content to be considered SS Alloy
10.5%
571: 2.1.17
Mtls – Minimum nickel content to be considered Nickel Alloy
> 30%
571: 2.1.16
AI – Amount of time inspector must be involved in inspection activities - required to maintain API 653 certification
20%
653: D.4.2.a
Reconstruction - % of weld intersections (new welds to old welds) to be RT’d
25%
653: 12.2.1.5
Linings – Max relative humidity when installing tank linings
80%
652: 8.3
NDE – Typical coverage of floor when performing MFL
80%
575: A.4
% to RT when installing a new insert plate with a nozzle into an existing shell plate
100%
653: 12.2.1.8