Scratch Resistant Coatings Flashcards
_ is benchmark material for abrasion resistance and optics
crown glass
scratched lenses have diminshed _
impact resistance
all non-glass materials are coated with SRC except _
CR-39 (naturally hard)
coated stock lenses are coated on which side(s)?
both sides
semifinished lenses are coated on which side(s)?
front surface only
SRCs are applied where? (2)
lens manufacturer
optical lab
if lens is AR coated, _ quality is essential to the success of AR
SRC
2 ways to apple SRC? (2)
thermally cured, UV cured
Thermally cured hard coatings are _ and removed _
For how long?
Commonly used by _
dipped; at consistent rate to control thickness
hours
manufacturers
UV cured hard coatings are applied how?
Cured for how long?
Commonly used by?
while it spins
seconds
labs
the type of material for SRC depends on whether or not _
the lens is to be tinted (difference between SRC and “hard coat”)
SRC = _$
hard coat= _$
20 (tintable)
40 (not-tintable)
although SRC are not designed to reduce lens reflections, they do exhibit some reduction in surface reflections
uncoated CR-39 transmits _%
SRC transmits _%
92
96
_ cannot accept tints
_ is part of lens that allows for tinting to occur
polycarbonate
SRC!!
SRC lenses should not be exposed to head, max _ degrees
- _ is preferred for making adjustments
200
air units