Cold Work - Increased (2)
Yield strength and tensile strength
Cold Work - Decreased (3)
strain to failure, ductility, electrical conductivity
Cold Work - No Change in ….
Young’s Modulus
Decrease in Re-crstytallization Temperature with _____ in Cold Work
Increase
Annealed (3 stages)
- Recovery
- Re-crystallization
- Growth
Annealed (opposite of ___ ____ properties)
Cold Work
How does Sintering work?
The powdered material is held in a mold and then heated to a temperature below the melting point.
The atoms in the powder particles diffuse across the boundaries of the particles, fusing the particles together and creating one solid piece.
Finer grain size means _____ in MOE
increase
Know the Dispersion Strengthing Phase Diagram
Check
Factors for effective Dispersion strengthing - The precipitate phase should be ___ and _______________
hard and discontinuous
Factors for effective Dispersion strengthing - The dispersed phase particles should be ____ and ________.
small and numerous.
Factors for effective Dispersion strengthing - The dispersed phase particles should be _____ rather than __________.
round rather than needlelike
Factors for effective Dispersion strengthing -Larger amounts of ______ _____ increase strengthening.
dispersed phase