application aids Flashcards

1
Q

Ca (s) used in process with V2O5

other than extracting vanadium, suggest one reason why this method is expensive?

A
  • calcium produced by electrolysis
  • uses large amount of energy
  • calcium is very reactive / reacts with air and so needs to be extracted
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
2
Q

pure vanadium produced along with HCl gas through the reaction with VCl and H2

identify 2 hazards

why is pure vanadium produced

A
  • hazards
    • HCl gas is toxic
    • explosion with hydrogen gas, it is flammible
  • only other product easily removed because it is a gas
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
3
Q

Antimony can be extracted by reacting scrap iron with low-grade ores that contain antimony sulfide (Sb2S3).

3Fe + Sb2S3 3FeS + 2Sb

Deduce one reason why the method of extraction of antimony from a low-grade ore, described in part (a), is a low-cost process. Do not include the cost of the ore.

A
  • uses cheap waste iron
  • single step process
    • uses less energy
How well did you know this?
1
Not at all
2
3
4
5
Perfectly