Abbreviations Flashcards
AI
Accumulation of
Imperfections
BT
Burn through
C
Cracks
CJP
Complete joint penetration
CP
Cluster Porosity
CFH
Cubic feet per hour
CSA
Cross sectional area
CVN
Charpy V-notch testing
EU
External undercut
ET
Eddy current testing
ID
Inside diameter
IF
Incomplete fusion
INCL
Inclusive
IP
Inadequate penetration without high low
IPD
Inadequate penetration do to High Low
IPM
Inches per minute
IU
Internal undercut
J
Joule
J/in
Joules per inch
LT
Leak testing
MT
Magnetic particle testing
NDE
Non destructive examination
NDT
Non destructive testing
NPS
Nominal pipe size
OD
Outside diameter
P
Porosity
PJP
Partial joint penetration
PQR
Procedure qualification record
PT
Penetrant testing
PWHT
Post weld heat treat
RT
Radiographic testing
TYP
Typical
UNS
Unified numbering system
UT
Ultrasonic testing
UTS
Ultimate tensile strength
VT
Visual testing
W
Width of bend specimen
WPS
Welding procedure specification
WQTR
Welder qualification test record