Past MCQ Flashcards

You may prefer our related Brainscape-certified flashcards:
1
Q

At what temp does feldspathic ceramic form leucite?

A
  • 1150-1500degrees C
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
2
Q

What is Leucite?

A
  • Potassium aluminium silicate
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
3
Q

What is PROCERA?

A
  • > 99% alumina core
  • Produced at about 1700 celcius
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
4
Q

What temp is Zirconia sintered at?

A
  • 1600C
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
5
Q

What is the max amount of strain porcelain will undergo before fracture?

A
  • 0.5%
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
6
Q

What is the expansion of gold ?

A
  • 1.4%
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
7
Q

What is the expansion of Ni/Cr?

A

2.0%

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
8
Q

What is the expansion of Co/Cr?

A

2.3%

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
9
Q

What is the longevity of GIC, SSC and Amalgam?

A

SSC = 92%
Amalgam = 80%
GIC = 66%

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
10
Q

What are the reasons and % for post core failures?

A
  • 60% due to restorative
  • 32% due to perio
  • 8% due to endo
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
11
Q

What are some temp materials used?

A

PMMA:Jet
PEMA: Snap / TRIM
Bis-acrylate composite : Protemp
UDMA : Provipont

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
12
Q

What material has best mechanical properties for restoration of occlusal surfaces?

A
  • Gold
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
13
Q

What is the best method for retaining a core ?

A
  • Use of adhesive only
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
14
Q

When preparing upper first permanent molar for metal-ceramic crown, a functional bevel is placed on which cusp?

A
  • Mesio-palatal
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
15
Q

What is the correct degree of axial-taper in ideal crown prep?

A
  • 7degrees
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
16
Q

The fit surface of a porcelain laminate veneers is prepared with what acid?

A
  • Hydrofluoric acid