non-skid Flashcards
Properly coded non-skid should have a surface profile of
1/3” min
1/16” max
Non-skid should be
9 inches
How many hours after primer has dried should the non-skid be applied
Within 36 hours
What is the shelf life of non-skid
1 year
Temperature of the deck to lay non-skid
55 degrees to 100 degrees
Composite G
Abrasive coating
Composite L
Non abrasive
How many inches do you extend to remove in damages non-skid
6 to 10 inches
Ambient air temp
55 to 100 degrees
What % of deck must be cleaned before priming the deck
95%
How far from deck fittings should you apply non-skid
2 inches
Service life of type 2, 3, 4composite G
6 months
Corrosion type that an ABH is mainly concerned with
Galvanic and surface
How many inches from coaming/ deck edge should you apply non-skid
5 inches
Max humidity for non-skid
85%
Temperature to store non-skid long term
55 to 100 degrees
What should the temperature be 24 hrs prior to mixing
70 to 80 degrees
High pressure blasting operated between
680 to 1700 bar
10000 to 25000 psi
What’s another name for the banana gauge
Magnetic dial gauge
Non-skid should be applied within how many hours after its laid
36 hours
How long does it take for primer to cure
6 to 12 hours
What’s is the NSTM 634
Deck covering
How long until non-skid is ready for foot traffic
24 hours
How long until non-skid is ready vehicular traffic
48 to 72 hours
How long until non-skid is ready fully operational
7 days