DATA Sheets- Misc Others Flashcards
Design- Two most common CS pipe materials
A53 and A106
NDE- Min angle of eye-to-part to count as visual exam
30 Degrees
Welding- Variables needed in WPS
Essential and Non Essential
NDE- Min light intensity when performing non-fluorescent MT or PT or VT exams
100 ft candles
Test- Max stress allowed during a pressure test
90% of SMYS
NDE- Min black light intensity when performing MT or PT fluorescent exams
1000 micro W /cm^2
Corrosion- Typical external corrosion rate for inland locations with moderate rain and humidity
1 - 3 mills per year
Welding- Variables needed in PQR
Essential
NDE- Weight used to check magnetic strength of an DC yoke
40 LBS
NDE- Two primary Gamma-ray RT sources
Iridium 192
Cobalt 60
NDE- Max UT scanning speed
6” per sec
Welding- Min taper required for welds with mismatch
30 degrees
Welding- Meaning of “S” in the electrode designation for a GMAW or GTAW electrode
Solid Wire
Repair- Max allowed SMYS for pipe if fillet- welded patch is installed
40,000 PSI
NDE- Hole size that must be visible in RT when using a hole-type IQI
2T