Amalgam Lecture Flashcards
Soupy, premature setting, brittle, excess matrix, difficult to remove amalgam says what about your trituration length?
It was overtriturated
Shiny, soft, warm amalgam says what about your trituration length?
It was properly triturated
Grainy, crumble, dull, excess Hg, reduced strength, hard to handle amalgam says what about your trituration length?
It was undertriturated
The process of compressing the alloy into the tooth prep and eliminating all voids
Condensation
Generally, condensation must be completed in ____ minutes otherwise cracks will be created
3-4
Pressure =
Force/Area
Small condenser -> higher pressure
Condensation must occurs under a wet or dry field?
Dry
If you feel you are perforating into the first increment of amalgam as you condense, then either:
- Your condensation force is too high
- You didn’t place enough increment
Last increment of amalgam should go beyond the external outline of the prep by ____ mm done with a ____ condenser
1.0 mm
Large condenser
Excess amalgam error that tapers beyond the external margin. Explorer catches from CSM to amalgam
Flash
Break/groove between tooth and amalgam restoration where food/microorganism can become trapped. (Operator error). Explorer catches from CSM to amalgam and vice versa
Open Margin Error
Amalgam does not reach enamel margin (operator error). Explorer catches from amalgam to CSM.
Submarginal/Ditching
Inadequate condensation can lead to this error
Void