XXXX Flashcards
1
Q
VT Examination
A
Eye within 6” to 24”
Angle the not less than 30 degrees
100 foot candles
2
Q
Plate conditioning
A
No more than 1/8”
3
Q
Recommended temperature during hydrostatic testing
A
At least 30F above the minimum design metal temperature, but need not to exceed 120F to minimize the risk of brittle fracture.