Oxyfuel Cutting Review Activity Flashcards
A ______ _____ can be used on a cast iron to cut it during demolition projects.
oxygen lance
A good standoff distance from the pre-heat cones to the plate is ______
1.6 mm - 3.2mm (1/16” - 1/8”)
Generally a ______ flame should be used for cutting.
neutral
Heat energy is expressed in ________
Megajoules per cubic metre (MJm3) or British Thermal Units per cubic foot (BTU/ft3)
If cutting materials 6” thick or greater a _____ torch is recommended.
Standard or Heavy duty cutting torch
If the inner flame cones are of different lengths, then _____
shut off the torch and clean or redrill the preheat orifices
If travel speed when cutting is too fast ______
slag will bubble up to the surface of the plate cause cutting jet stream cannot blow through the full thickness of the material.
On a combination torch, the torch handle oxygen valve should be _______ when lighting the torch.
Fully opened
Rapid oxidation occurs when steels are heated to their kindling point of _______ and a jet stream of high-pressure oxygen is directed onto the hot spot
760c - 870c (1400f - 1600f)
Should you leave a radiograph of pipe beveller unattended when cutting?
Never
The most popular torch unit is _____
combination welding and cutting torch`
The recommended oxygen and acetylene pressures for a #1 tip are ______
oxygen pressure 30 psi and acetylene pressure 3 psi
The slag when cutting will collect _______
on the piece that the tip is pointing at
The ________ tip is good for removing minor imperfections during foundry and casting work.
scarfing
Thinner materials require _____ inclination
more forehand