API 572 Flashcards
3.1.29 temper embrittlement occurs for low alloy steel from exposure to temperatures ranging:
650 to 100 degrees F
9.1 Is it mandatory to remove internal/external coverings for inspection
no
9.2.1 the primary method for obtaining thickness measurements
UT
9.3.8 which technique is used to scan guy wires
AUT (automated ultrasonic technique)
9.3.10 Recommended grounding resistance should be less than:
5 ohms
9.3.10 maximum grounding resistance is
25 ohms
9.3.14 Most severe soil corrosion will be found:
ground level and several inches below
9.3.14 hydrogen blistering is typically found
on the inside of a vessel containing acid
9.4.4.3 What is characterized by a smooth, bright appearance?
errosion
9.4.4.3 What is not characterized by smooth bright appearance?
corrosion
9.4.6 Ring joint flanges should be inspected for:
cracks due to excessive bolt tightening