As per API 650, ,,,,,, type of steel is not permitted
Rimmed or capped
As per API 650, Use of cast iron for any pressure part or any part attached to the tank by welding is ,,,,,
prohibited
Because of hydrogen embrittlement and toxicity concerns, ,,,,,, components shall not be used without the expressed consent of the Purchaser
cadmium-plated
Any new or unused plate and pipe material cannot be completely identified by records that may be used in the construction of tanks, if the material passes the tests
Each plate shall be subjected to the chemical analysis and physical tests
Plates:
The edge thickness ordered shall ,,,,,,, than the computed design thickness or the minimum
permitted thickness
not be less
Plates:
Incoming plate material shall not be under run, more than ,,,,, from design thickness
0.3 mm (0.01”)
Plates:
All plates shall be manufactured by the,,,,,,or ,,,,,, process
- Open-hearth, Electric-furnace,
- Basic oxygen
Plates:
Shell plates are limited to a maximum thickness of ,,,,,
45 mm (1.75 in.)
Plate:
When specified by the plate purchaser, the steel shall be ,,,,,. When specified by the plate purchaser,
fully killed
Plates:
fully killed steel shall be made to ,,,,,practice.
fine-grain
Plates:
fully killed plates shall be heat treated to produce grain refinement by either ,,,, or ,,,,, for hot forming
normalizing
heating uniformly
Plates: (Impact Testing)
An impact test shall be performed on ,,,,, specimens taken from a single test coupon or test location
three
Plates: (Impact Testing)
If more than one value is less than the specified minimum value, ,,,,,, additional specimens shall be tested
three
Plates: (Impact Testing)
The min. Avg Value of impact test three specimen shall not b less then ,,,,,,,for longitudinal specimens and,,,,,,,,,,,transverse speciemns
18 J or ( 15 ft-lbf )
20 J or ( 13 ft-lbf )
Structural Material:
Structural steel shall conform to
ASTM A36 / A992